As the number of ceramic THR bearings used worldwide is increasing, the number of implants that experience off-normal working conditions, e.g. edge loading, third bodies in the joint, soft tissues laxity, dislocation/subluxation of the joint, increases too. Under all such conditions the bearing surfaces can be damaged, leading eventually to a limitation of the expected performances of the implant. We characterised the damage resistance of different bearing surfaces (alumina matrix composite BIOLOXdelta, alpha-alumina BIOLOXforte, zirconia 3Y-TZP, oxidized zirconium alloy Zr-2.5Nb, CoCr-alloy) by scratch tests performed following the European standard EN 1071–3:2005. Also the scratch hardness of same materials has been assessed.Background
Methods