Please check your email for the verification action. You may continue to use the site and you are now logged in, but you will not be able to return to the site in future until you confirm your email address.
Introduction. Concerns regarding UHMWPE wear particle induced osteolysis in total hip replacement(THR, [1]) have led to alternative materials to be sought. Carbon-fibre reinforced poly-ether-ether-ketone (CFR-PEEK) has shown reduced wear in hip and knee configurations compared with conventional polyethylene [2-4]. The aim of this study was to investigate the wear performance of a ceramic-on-CFR PEEK THR through a simulator study. Methodology. Five 36mm diameter Biolox Delta heads were paired with extruded CFR-PEEK cups and tested in a hip wear simulator (Simulator Solutions, UK) for 10 million cycles (Mc). Tests were performed in a Prosim hip simulator, which applied a twin peak loading cycle, with a peak load of 3kN. Flexion-extension of −15 to +30 degrees was applied to the head and internal-external rotation of +/− 10 degrees was applied to the cup, components were mounted anatomically. The lubricant was 25% (v/v) calf serum supplemented with 0.03% (w/v) sodium azide. Wear was assessed gravimetrically at several intervals adjusted for moisture uptake using loaded and unloaded soak controls. Results. The volumetric wear of the CFR-PEEK cups was calculated from weight loss, corrected for fluid uptake by a mean value of the loaded and unloaded soak controls. The CFR-PEEK bearings exhibited step-like wear behaviour throughout the study (Figure 1), with periods of ‘higher’ wear rate (between 0.4mm–1.4mm. 3. /Mc) and periods of a ‘lower’ wear rate (less than 0.4mm. 3. /Mc), a phenomenon that has previously been observed with this material [3]]). Discussion. The wear of a novel ram-extruded CFR-PEEK cup, articulating with a Biolox Delta ceramic head was assessed through a 10Mc experimental wear study. The mean wear rate over the period of the study was very low, with less than 1mm. 3. /Mc measured. The wear rates observed in this study are comparable with reported wear rates for 36mm diameter hard-on-hard bearings [5], and lower than wear rates measured for a highly cross-linked polyethylene bearing [6]. The wear rates reported in this study are lower than those previously reported [3], however, as CFR-PEEK operates within a boundary lubrication regime, the reduced head diameter in the present study would result in reduced sliding distance and lower surface wear